Technical Support
BGA CHIPSET OBSERVE PRECAUTIONS FOR HANDLING
BGA Chips is MOISTURE SENSITIVE DEVICES. Devices require baking, before mounting, Here is the general bake-out process, Lay the BAG on the tray, and put it in to a baking dry cabinet. Set the temperature and time as: 125C x 24 hours or 80C x 48 hours
Pay attention to the difference between
leaded (Pb) balls and lead free (No Pb) balls.
Lead-free/No Pb BGA chips:
245C-260C(Maximun)
Leaded/Pb BGA chips:
180C-205C(Maximun)
Sufficient Stock
No customer reviews for the moment.
16 other products in the same category
SRCKB SRCUU SRD1V SREJP SREJQ SREJR SRF6X SRFFX SRFFZ SRGKW 8265U 8565U Stencil Template 90x90
Brands: Chipsetpro.com
€23.00
SRCKB SRCUU SRD1V SREJP SREJQ SREJR SRF6X SRFFX SRFFZ SRGKW 8265U 8565U Stencil Template 90*90
GTX1060 N17EG1A1 Stencil Template 90x90
Brands: Chipsetpro.com
€9.97
GTX1060 N17E-G1-A1 Stencil Template 90*90
BD82HM70 SJTNV Stencil Template 90x90
Brands: Chipsetpro.com
€9.96
BD82HM70 SJTNV Stencil Template 90*90